具有异常放热现象的Fe-Nb-B-Y非晶合金燃烧机理 |
| 胡祥, 葛嘉城, 刘思楠, 伏澍, 吴桢舵, 冯涛, 刘冬, 王循理, 兰司 |
|
Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon |
| HU Xiang, GE Jiacheng, LIU Sinan, FU Shu, WU Zhenduo, FENG Tao, LIU Dong, WANG Xunli, LAN Si |
| 图3 Y4.5块体非晶合金在同步辐射原位加热实验中出现的自放热现象 (a) heating process (b) heating rate |
| Fig.3 A self-heating process of the Y4.5 bulk metallic glasses during the in situ synchrotron HE-XRD experiment upon heating (The self-heating rate is 24.4 K/s) |
|