具有异常放热现象的Fe-Nb-B-Y非晶合金燃烧机理 |
| 胡祥, 葛嘉城, 刘思楠, 伏澍, 吴桢舵, 冯涛, 刘冬, 王循理, 兰司 |
|
Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon |
| HU Xiang, GE Jiacheng, LIU Sinan, FU Shu, WU Zhenduo, FENG Tao, LIU Dong, WANG Xunli, LAN Si |
| 图1 Fe-Nb-B-Y非晶合金在空气中的点火和燃烧过程光学摄像记录照片 (a) 0 s (b) 1 s (c) 2 s (d) 3 s (e) 4 s (f) 5 s |
| Fig.1 The video snapshots by an optical camera of combustion phenomenon for Fe-Nb-B-Y metallic glasses (MGs) in air showing Y4.5 ribbon has the fastest burning rate compared to Y3 and Y7 MGs, while Y0 cannot finish self-propagating combustion |
|