块体非晶合金的3D打印成形研究进展
|
|
李宁, 黄信
|
Recent Advances on 3D Printed Bulk Metallic Glasses
|
|
LI Ning, HUANG Xin
|
|
表1 3D打印成形块体非晶合金与原材料的相组成[12,14,16,17,21~55]
|
Table 1 Summaries of the phase features of 3D-printed BMGs with its original feedstocks[12,14,16,17,21-55]
|
|
Composition (atomic fraction / %) | Feedstock | 3D printed sample | Technique | Ref. |
|---|
| | | |
|---|
| Fe43.7Co7.3Cr14.7Mo12.6C15.5B4.3Y1.9 | Amorphous | Amorphous | SLM | [24] | | Fe37.5Cr27.5Mo10C12B13 | | | SLM | [27,28] | | Fe68.3C6.9Si2.5B6.7P8.7Cr2.3Mo2.5Al2.1 | | | SLM | [29] | | Fe55Cr25Mo16B2C2 | | | SLM | [30] | | Zr60.14Cu22.31Fe4.85Al9.7Ag3 | | | SLM | [31,32] | | Zr52.5Cu17.9Ni14.6Al10Ti5 | | | SLM | [33] | | Zr52.5Ti5Al10Ni14.6Cu17.9 | | | LFP | [34] | | Zr65Cu17.5Ni10Al7.5 | | | LFP | [25] | | Zr44Ti11Cu10Ni10Be25 | | | FFF | [16] | | Fe48C15B6Mo14Cr15Y2 | | | TS3DP | [17] | | Cu47Ti33Zr11Ni8Si1 | Amorphous | Amorphous + crystalline | LENS | [35] | | Fe71Si10B11C6Cr2 | | | SLM | [36] | | Zr55Cu30Al10Ni5 | | | SLM | [22,37] | | Zr60Fe10Cu20Al10 | | | SLM | [38] | | Zr59.3Cu28.8Nb1.5Al10.4 | | | SLM | [39,40] | | Al86Ni6Y4.5Co2La1.5 | | | SLM | [21] | | Cu50Zr43Al7 | | | SLM | [41] | | Cu46Zr47Al6Co1 | | | SLM | [42] | | Zr52.5Ti5Al10Ni14.6Cu17.9 | | | SLM | [43] | | Zr51Ti5Cu25Ni10Al9 | | | LENS | [44,45] | | Zr50Ti5Cu27Ni10Al8 | | | LENS | [46] | | Fe58Cr15Mn2B16C4Mo2Si1W1Zr1 | Amorphous + crystalline | Amorphous + crystalline | LENS | [14] | | Zr55Cu30Al10Ni5 | | | LENS | [47,48] | | Zr39.6Ti33.9Nb7.6Cu6.4Be12.5 | | | LENS | [49] | | Fe74Mo4P10C7.5B2.5Si2 | | | SLM | [12] | | Fe70Cr5Ni3Mo3W9Si5B5 | | | SLM | [50] | | Zr57.4Ni8.2Cu16.4Ta8Al10 | | | SLM | [51] | Fe38Ni30-xSi16B14V2Mx (M contains Al, Ti, Mo, and C) | | | LENS | [52] | | | | | | Fe54.35Cr18.47Mn2.05Mo13.93W5.77B3.22C0.90Si1.32 | Amorphous + crystalline | Amorphous | SLM | [53] | | Ti47Cu38Zr7.5Fe2.5Sn2Si1Ag2 | | | SLM | [23] | | Al85Ni5Y6Co2Fe2 | Amorphous + crystalline | Fully crystallized | SLM | [54] | | Fe41Co7Cr15Mo14C15B6Y2 | | | FDM | [55] |
|
|
|