块体非晶合金的3D打印成形研究进展
李宁, 黄信

Recent Advances on 3D Printed Bulk Metallic Glasses
LI Ning, HUANG Xin
图11 SLM成形的Zr59.3Cu28.8Nb1.5Al10.4样品疲劳裂纹扩展实验结果[64]
Fig.11 Fatigue crack-growth testing results for SLM processed Zr59.3Cu28.8Nb1.5Al10.4 samples[64]K represents stress intensity range, ΔKth represents threshold stress intensity range, ΔKmax represents the maximum stress intensity range)