块体非晶合金的3D打印成形研究进展 |
| 李宁, 黄信 |
|
Recent Advances on 3D Printed Bulk Metallic Glasses |
| LI Ning, HUANG Xin |
| 图10 按比例混合了Cu、CuNi20和CuNi30粉末的SLM成形样品的应力-应变曲线和通过引入第二相后SLM成形铁基非晶合金的力学性能变化情况[ |
| Fig.10 Compressive stress-strain curves of SLM processed specimens by mixing Cu powder (20%, 35% and 50%, mass fraction), CuNi20, and CuNi35 powders (50%, mass fraction), respectively (a) and mechanical properties of SLM processed Fe-based BMG composites by tuning the content or category of the second phase (b)[ |
|