块体非晶合金的3D打印成形研究进展 |
| 李宁, 黄信 |
|
Recent Advances on 3D Printed Bulk Metallic Glasses |
| LI Ning, HUANG Xin |
| 图9 SLM成形锆基非晶圆柱与铸态非晶压缩曲线[ |
| Fig.9 Compressive stress-strain curves of the SLM Zr-based BMG rods,as compared with the as-cast one (σmax—maximum stress)[ |
|