块体非晶合金的3D打印成形研究进展 |
| 李宁, 黄信 |
|
Recent Advances on 3D Printed Bulk Metallic Glasses |
| LI Ning, HUANG Xin |
| 图7 非晶与铜界面处的TEM分析[ |
| Fig.7 TEM micrograph shows the interface between amorphous lamellae and Cu lamellae, the inserts demonstrate the glassy and fcc microstructure (a), HRTEM image of region “B” that contains nanocrystals (b), EDS profiles along line “C” cross the boundary (c), and high-density dislocations formed in the Cu crystals (d)[ |
|