块体非晶合金的3D打印成形研究进展 |
| 李宁, 黄信 |
|
Recent Advances on 3D Printed Bulk Metallic Glasses |
| LI Ning, HUANG Xin |
| 图5 Zr52.5Cu17.9Ni14.6Al10Ti5粉末、铸态样品和不同激光能量密度下SLM成形样品的XRD谱、激光能量密度13 J/mm3时3D打印样品的同步辐射实验及衍射图样[ |
| Fig.5 X-ray diffraction patterns of the Zr52.5Cu17.9Ni14.6Al10Ti5 powder, an as-cast rod and SLM samples produced with varying energy densities (a), synchrotron experiments for sample 3D printed under 13 J/mm3 (b), and diffraction patterns wherein no indication of the presence of crystals and the structure is fully amorphous regardless the position (c) (E represents energy density)[ |
|