块体非晶合金的3D打印成形研究进展 |
| 李宁, 黄信 |
|
Recent Advances on 3D Printed Bulk Metallic Glasses |
| LI Ning, HUANG Xin |
| 图3 Zr55Al10Ni5Cu30 非晶合金粉体经激光表面熔覆不同次数的微观结构、熔覆1~7层的截面微结构、熔覆20次后的SEM像和沉积7层的SEM像[ |
| Fig.3 Microstructures of the Zr55Al10Ni5Cu30 BMGs by pulsed laser surface melting (PLSM) with one, six, twelve and twenty pulsed laser irradiations (a), microstructures of the deposits with one, two, four and seven layers (b), SEM image of twenty times irradiations (c), and SEM image of seven deposited layers (d)[ |
|