块体非晶合金的3D打印成形研究进展 |
| 李宁, 黄信 |
|
Recent Advances on 3D Printed Bulk Metallic Glasses |
| LI Ning, HUANG Xin |
| 图2 熔池区(P1)、热影响区(P2)和无相变区(P3)的热过程曲线以及热影响区中不同位置的热过程曲线[ |
| Fig.2 Heating-cooling curves in the MP (P1), HAZ (P2) and un-affected zone (P3) (a) and heating-cooling curves in the different locations of HAZ (b) (MP—molten pool, HAZ—heat affected zone, Tm represents melting temperature, Tg represents glass transition temperature, Tx represents crystallization temperature)[ |
|