块体非晶合金铸造成形的研究新进展 |
| 刘日平, 马明臻, 张新宇 |
|
New Development of Research on Casting of Bulk Amorphous Alloys |
| LIU Riping, MA Mingzhen, ZHANG Xinyu |
| 图4 在1353 K下铸造的钥匙的SEM像[ (a) taken at the core of the key, showing a completely crystalline region (b) taken between the core and the outer surface, revealing the interface between the glassy and crystalline parts (c) taken close to the outer surface, showing a completely glassy part of the key |
| Fig.4 SEM images of the key cast at 1353 K[ |
|