块体非晶合金铸造成形的研究新进展 |
| 刘日平, 马明臻, 张新宇 |
|
New Development of Research on Casting of Bulk Amorphous Alloys |
| LIU Riping, MA Mingzhen, ZHANG Xinyu |
| 图3 高压铸造装置示意图、模具的三维模型及由耐热钢和铜合金制成的铸造模具[ |
| Fig.3 Schematic illustration of the high pressure die casting setup (a), 3D model of the die (b), and completed dies made from heat resistant steel and a copper alloy (c, d)[ |
|