金属玻璃结构及其失稳的原子层次研究 |
| 管鹏飞, 孙胜君 |
|
Atomic-Level Study in the Structure and Its Instability of Metallic Glasses |
| GUAN Pengfei, SUN Shengjun |
| 图9 基于温度-应力空间的宏观动力学相图,由黏度定义了金属玻璃的玻璃态和流变态[ |
| Fig.9 Two-dimensional plot of viscosity as a function of temperature and stress in a model metallic glass (T0 = 860 K, σ0—the critical stress where η0 diverges in extrapolation to T = 0?K, σ—stress, η—viscosity, η0—the viscosity to define the glass transition)[ |
|