金属玻璃中的非晶多形态转变 |
| 曾桥石, 尹梓梁, 楼鸿波 |
|
Polyamorphic Transitions in Metallic Glasses |
| ZENG Qiaoshi, YIN Ziliang, LOU Hongbo |
| 图6 Ce68Al10Cu20Co2金属玻璃的弹性常数和Poisson比随压力的变化[ |
| Fig.6 Bulk modulus (a), shear modulus (b), Poisson's ratio (c), and Young's modulus (d) of the Ce68Al10-Cu20Co2 metallic glass as a function of pressure (Arrows indicate the critical pressures of the polyamorphic transition)[ |
|