金属玻璃中的非晶多形态转变 |
| 曾桥石, 尹梓梁, 楼鸿波 |
|
Polyamorphic Transitions in Metallic Glasses |
| ZENG Qiaoshi, YIN Ziliang, LOU Hongbo |
| 图5 Yb62.5Zn15Mg17.5Cu5金属玻璃的电阻随压力的变化关系[ |
| Fig.5 Relative resistance of the Yb62.5Zn15Mg17.5Cu5 metallic glass as a function of pressure (The inset shows the microphotograph of the sample with four Pt electrodes in chamber between two anvils at about 5 GPa conditions. Rp—resistance at high pressure, R0—resistance at 0 GPa, LDAS—low-density amorphous state, HDAS—high-density amorphous state)[ |
|