物理气相沉积制备金属玻璃薄膜及其力学性能的样品尺寸效应 |
| 曹庆平, 吕林波, 王晓东, 蒋建中 |
|
Magnetron Sputtering Metal Glass Film Preparation and the “Specimen Size Effect” of the Mechanical Property |
| CAO Qingping, LV Linbo, WANG Xiaodong, JIANG Jianzhong |
| 图10 Ni-Nb金属玻璃薄膜密度和弹性应变极限随薄膜厚度的变化[ |
| Fig.10 Density and elasticity of Ni-Nb metallic glass thin films vary with film thickness[ |
|