物理气相沉积制备金属玻璃薄膜及其力学性能的样品尺寸效应 |
| 曹庆平, 吕林波, 王晓东, 蒋建中 |
|
Magnetron Sputtering Metal Glass Film Preparation and the “Specimen Size Effect” of the Mechanical Property |
| CAO Qingping, LV Linbo, WANG Xiaodong, JIANG Jianzhong |
| 图1 Zr-Cu-Al超稳定金属玻璃薄膜、淬火薄带以及不同温度退火90 h后的DSC曲线,及基底温度对玻璃化转变温度(Tg)变化的影响[ |
| Fig.1 DSC curves of Zr-Cu-Al ultrastable metallic glass thin films (SMG), quenched ribbons metallic glass (MG) and after annealing at different temperatures for 90 h (a), and influence of substrate temperature (Tsub) on the glass transition temperature (Tg) as compared with that of quenched metallic glass ribbon (Tg, quenched) (b) (δTg represents temperature difference between Tg and Tg, quenched)[ |
|