金属玻璃的剪切带变形与断裂机制研究进展 |
| 屈瑞涛, 王晓地, 吴少杰, 张哲峰 |
|
Research Progress in Shear Banding Deformation and Fracture Mechanisms of Metallic Glasses |
| QU Ruitao, WANG Xiaodi, WU Shaojie, ZHANG Zhefeng |
| 图14 金属玻璃的缺口拉伸变形断裂形貌及其缺口强度比与其他合金的对比[ |
| Fig.14 Notch tensile deformation (a, b) and fracture (c) morphologies of a Zr-based MG, and comparison of notch strength ratio between MGs and other alloys (d) (σN—the nominal ultimate tensile stress (UTS) of notched specimen, σT—the UTS of smooth specimen)[ |
|