金属玻璃的剪切带变形与断裂机制研究进展 |
| 屈瑞涛, 王晓地, 吴少杰, 张哲峰 |
|
Research Progress in Shear Banding Deformation and Fracture Mechanisms of Metallic Glasses |
| QU Ruitao, WANG Xiaodi, WU Shaojie, ZHANG Zhefeng |
| 图11 金属玻璃循环压缩过程中剪切带演化及疲劳裂纹长度随加载周次增加的变化关系[ |
| Fig.11 Evolution of shear band and variation of fatigue crack length with increasing cyclic number during cyclic compression of an MG[ |
|