金属玻璃的剪切带变形与断裂机制研究进展 |
| 屈瑞涛, 王晓地, 吴少杰, 张哲峰 |
|
Research Progress in Shear Banding Deformation and Fracture Mechanisms of Metallic Glasses |
| QU Ruitao, WANG Xiaodi, WU Shaojie, ZHANG Zhefeng |
| 图10 在不同加载周数下剪切带局部剪切位移(λ)和不同位置(δ)的关系[ |
| Fig.10 Local shear offset as a function of the distance from the origin site of shear band for one shear band after different loading cycles[ |
|