金属玻璃的剪切带变形与断裂机制研究进展 |
| 屈瑞涛, 王晓地, 吴少杰, 张哲峰 |
|
Research Progress in Shear Banding Deformation and Fracture Mechanisms of Metallic Glasses |
| QU Ruitao, WANG Xiaodi, WU Shaojie, ZHANG Zhefeng |
| 图2 钛基金属玻璃的工程应力-工程应变曲线在宏观屈服附近的局部放大图[ |
| Fig.2 Magnified engineering stress-strain curve of Ti-based metallic glass (MG) close to the macroscopic yielding point (MYP) (Insets illustrate the inserting and transecting shear bands in the MG samples)[ |
|