非晶合金的回春行为 |
| 潘杰, 段峰辉 |
|
Rejuvenation Behaviors in Metallic Glasses |
| PAN Jie, DUAN Fenghui |
| 图3 三维应力状态压缩法实现非晶合金的剧烈回春[ (a) triaxial stress state was introduced in a circumferential notched BMG (b) DSC traces of as-cast and notched BMGs with 40% plastic strain |
| Fig.3 Rejuvenation of bulk metallic glass (BMG) through triaxial compression[ |
|