金属玻璃的结构年轻化及其对力学行为的影响 |
| 蒋敏强, 高洋 |
|
Structural Rejuvenation of Metallic Glasses and Its Effect on Mechanical Behaviors |
| JIANG Minqiang, GAO Yang |
| 图5 2种Cu-Zr金属玻璃在弹性静态压缩加载情况下加载时间对年轻化的影响[ |
| Fig.5 Influence of loading time on rejuvenation of two Cu-Zr metallic glasses under elastostatic compression[ |
|