高熵合金中的局域化学有序 |
| 丁俊, 王章洁 |
|
Local Chemical Order in High-Entropy Alloys |
| DING Jun, WANG Zhangjie |
| 图7 局域化学有序的强化效应[ (a) correlation between nanoscale segment detrapping events and spatial deviations from chemical disorder (Atoms are colored according to the coarse-grained α (b) LCO-induced strengthening (The average activation barriers, activation volume as well as activation stress associated with the nanoscale segment detrapping process; RSS is for random solid solution and Ta represents the temperature for Monte Carlo simulation) |
| Fig.7 Strengthening induced by local chemical order[ |
|