高熵合金中的局域化学有序 |
| 丁俊, 王章洁 |
|
Local Chemical Order in High-Entropy Alloys |
| DING Jun, WANG Zhangjie |
| 图6 CoCrFeMnNi块体多晶试样变应变速率拉伸测试[ (a) tensile true stress and true strain (b) strain-dependent activation volume of dislocation slip (b—module of Burgers vector) |
| Fig.6 Tensile test of polycrystalline CoCrFeMnNi high-entropy alloy[ |
|