高熵合金中的局域化学有序 |
| 丁俊, 王章洁 |
|
Local Chemical Order in High-Entropy Alloys |
| DING Jun, WANG Zhangjie |
| 图5 高熵合金与局域化学有序相关的位错行为[ (a) water-quenched (b) aged at 1000oC |
| Fig.5 Planar dislocations slip influenced by local chemical order in CrCoNi alloys[ |
|