高熵合金中的局域化学有序 |
| 丁俊, 王章洁 |
|
Local Chemical Order in High-Entropy Alloys |
| DING Jun, WANG Zhangjie |
| 图4 局域化学有序对CrCoNi合金层错能的影响[ (a) atomic configuration of stacking fault in CrCoNi alloy[ (b) the distribution of stacking fault energies (γisf) in CrCoNi alloys with a variety of local chemical order (from random solid solution CH_0, to the highest degree, CH_F), measured by DFT (density function theory) calculation[ (c) low angle annular dark field (LAADF) images showing dislocation dissociations in water-quenched and 1000oC aged samples, respectively[ (d) distribution of the measured separation of partial dislocation pairs from both water-quenched and 1000oC aged samples[ |
| Fig.4 Effect of local chemical order on the stacking fault energies in CrCoNi alloys |
|