纳米晶合金热稳定性的熵调控设计 |
| 王一涵, 原园, 喻嘉彬, 吴宏辉, 吴渊, 蒋虽合, 刘雄军, 王辉, 吕昭平 |
|
Design for Thermal Stability of Nanocrystalline Alloys Based on High-Entropy Effects |
| WANG Yihan, YUAN Yuan, YU Jiabin, WU Honghui, WU Yuan, JIANG Suihe, LIU Xiongjun, WANG Hui, LU Zhaoping |
| 图4 450℃等温热处理下不同晶粒尺寸FeCoNiCrMn合金的的Young's模量与硬度,以及各阶段的三维原子探针形貌演变图[ |
| Fig.4 Room-temperature hardness, Young's modulus, and APT reconstructions of FeCoNiCrMn alloys with different grain sizes after isothermal heat treatments at 450oC for various time[ |
|