纳米晶合金热稳定性的熵调控设计 |
| 王一涵, 原园, 喻嘉彬, 吴宏辉, 吴渊, 蒋虽合, 刘雄军, 王辉, 吕昭平 |
|
Design for Thermal Stability of Nanocrystalline Alloys Based on High-Entropy Effects |
| WANG Yihan, YUAN Yuan, YU Jiabin, WU Honghui, WU Yuan, JIANG Suihe, LIU Xiongjun, WANG Hui, LU Zhaoping |
| 图1 从单晶金属到纳米晶合金再到纳米晶高熵合金的结构示意图[ |
| Fig.1 Microstructural schematic of the progression from single crystal metal to nanocrystalline (NC) metal to NC-HEA (HEA—high-entropy alloy)[ |
|