高熵合金中的元素分布规律及其作用 |
| 余倩, 陈雨洁, 方研 |
|
Heterogeneity in Chemical Distribution and Its Impact in High-Entropy Alloys |
| YU Qian, CHEN Yujie, FANG Yan |
| 图4 bcc类高熵合金中的元素分布均匀性及其位错行为[ (a) dislocation structures in HfNbTaTiZr HEAs[ (b) dislocation structures in Ti38V15Nb23Hf24[ (c) short-range clustering structure in HfNbTaZr after annealing[ (d) ordered oxygen complexes regions in TiZrHfNb with 2% oxygen[ |
| Fig.4 Heterogeneity in chemical distribution and corresponding dislocation behaviors in bcc HEAs |
|