高熵合金中的元素分布规律及其作用 |
| 余倩, 陈雨洁, 方研 |
|
Heterogeneity in Chemical Distribution and Its Impact in High-Entropy Alloys |
| YU Qian, CHEN Yujie, FANG Yan |
| 图1 传统固溶体模型与高熵合金中的元素分布模型 (a) random solid solution (b) two kinds of inhomogeneity of element distribution: concentration wave and short-range order (c) dislocation slip energy barrier model in random solid solution (d) dislocation slip energy barrier in HEAs |
| Fig. 1 The model of traditional solid solution and the inhomogeneity of element distribution in high-entropy alloys (HEAs) |
|