基于第一性原理的金属导热性能研究
崔洋1, 李寿航2, 应韬1(), 鲍华2, 曾小勤1
Research on the Thermal Conductivity of Metals Based on First Principles
CUI Yang1, LI Shouhang2, YING Tao1(), BAO Hua2, ZENG Xiaoqin1

图3. Al、Mg和Zn的电导率计算值与实测值[26~28]随温度变化关系

Fig.3. Comparisons of the relationships between calculated and measured[26~28] electrical conductivities of Al, Mg, and Zn with temperature (T)