GH4169合金与S31042钢线性摩擦焊接头组织及力学性能
|
|
Microstructure and Mechanical Properties of Linear Friction Welding Joint of GH4169 Alloy/S31042 Steel
|
|
图9. S3102钢一侧热力影响区至焊缝区显微组织的TEM像 |
Fig.9. TEM images of S31042 steel from thermo-mechanically affected zone to weld zone |
![]() |