GH4169合金与S31042钢线性摩擦焊接头组织及力学性能
|
李彦默 1,2, 郭小辉 1, 陈斌 1, 李培跃 1, 郭倩颖 2, 丁然 2, 余黎明 2(  ), 苏宇 3, 李文亚 3
|
|
Microstructure and Mechanical Properties of Linear Friction Welding Joint of GH4169 Alloy/S31042 Steel
|
LI Yanmo 1,2, GUO Xiaohui 1, CHEN Bin 1, LI Peiyue 1, GUO Qianying 2, DING Ran 2, YU Liming 2(  ), SU Yu 3, LI Wenya 3
|
|
|
图8. S31042/GH4169线性摩擦焊接头焊缝区和热力影响区的EBSD图 Color online (a) misorientation distribution (High angle grain boundaries with misorientation angles over 15° are represented by black lines, and low angle grain boundaries with misorientation angles lower than or equal to 15° are represented by red lines)(b) inverse pole figure(c) Kernel average misorientation (KAM)
|
Fig.8. EBSD maps of weld zone and thermo-mechanically affected zone of S31042/GH4169 linear friction welded joint
|
|
 |
|
|