GH4169合金与S31042钢线性摩擦焊接头组织及力学性能
|
李彦默 1,2, 郭小辉 1, 陈斌 1, 李培跃 1, 郭倩颖 2, 丁然 2, 余黎明 2(  ), 苏宇 3, 李文亚 3
|
|
Microstructure and Mechanical Properties of Linear Friction Welding Joint of GH4169 Alloy/S31042 Steel
|
LI Yanmo 1,2, GUO Xiaohui 1, CHEN Bin 1, LI Peiyue 1, GUO Qianying 2, DING Ran 2, YU Liming 2(  ), SU Yu 3, LI Wenya 3
|
|
|
图5. S31042钢一侧不同区域显微组织的SEM像 (a) near-weld line thermo-mechanically affected zone (b) far-weld line thermo-mechanically affected zone (c) heat affected zone (d) parent metal
|
Fig.5. SEM images of various zones in S31042 steel
|
|
 |
|
|