GH4169合金与S31042钢线性摩擦焊接头组织及力学性能
李彦默1,2, 郭小辉1, 陈斌1, 李培跃1, 郭倩颖2, 丁然2, 余黎明2(), 苏宇3, 李文亚3
Microstructure and Mechanical Properties of Linear Friction Welding Joint of GH4169 Alloy/S31042 Steel
LI Yanmo1,2, GUO Xiaohui1, CHEN Bin1, LI Peiyue1, GUO Qianying2, DING Ran2, YU Liming2(), SU Yu3, LI Wenya3

图2. S31042/GH4169线性摩擦焊接头显微组织的OM像

Fig.2. OM image of S31042/GH4169 linear friction welded joint (A—weld zone, B—near-weld line thermo-mechanically affected zone, C—far-weld line thermo-mechanically affected zone, D—heat affected zone, E—parent metal)