| Taylor factor M | 3.06 | Present model |
| Coherency strain for η'εη' | 0.0133 | Present model |
| Coherency strain for GPI εGPI | 0.0025 | Present model |
| Constant depends on the precipitation κ | 3.2 | Present model |
| Maximum volume fraction of whole precipitation | 0.1035 | Ref.[13] |
| Maximum volume fraction of the GPI zone | 0.025 | Present model |
| Shear modulus G | 27 GPa | Ref.[25] |
| Shear modulus between the η' and matrix ΔEη' | 0.7 GPa | Ref.[26] |
| Shear modulus between the GPI zones and matrix ΔEGPI | 1.5 GPa | Present model |
| Inherent strength of Al σi | 15.7 MPa | Ref.[27] |
| Grain boundary strengthening value ΔσGB | 22 MPa | Present model |
| Constant depends on the solute atoms C3 | 237.5 MPa | Present model |
| Magnitude of the Burgers vector b | 0.286 nm | Ref.[25] |