AA 7055铝合金时效析出强化模型
陈军洲1,2(), 吕良星3, 甄良3, 戴圣龙1,2
Precipitation Strengthening Model of AA 7055 Aluminium Alloy
CHEN Junzhou1,2(), LV Liangxing3, ZHEN Liang3, DAI Shenglong1,2

图13. AA 7055铝合金120℃欠时效模型屈服强度预测值(式(46))与实验值的比较

Fig.13. Yield strength from the experiment compared with the predicted value using under-aged model (Eq.(46)) for the AA 7055 Al alloy aged at 120oC