AA 7055铝合金时效析出强化模型
|
|
Precipitation Strengthening Model of AA 7055 Aluminium Alloy
|
|
图9. AA 7055铝合金160℃整个时效阶段屈服强度预测值(式(43))与实验值的比较 |
Fig.9. Yield strength from the experiment compared with the model predicted (Eq.(43)) for the AA 7055 Al alloy aged at 160oC |
![]() |