690 MPa级高强韧低碳微合金建筑结构钢设计及性能
|
|
Design and Performance of 690 MPa Grade Low-Carbon Microalloyed Construction Structural Steel with High Strength and Toughness
|
|
图11. TMCP处理的实验用钢在1/4厚度处析出物形貌的TEM像 |
Fig.11. TEM images of the tested steel at 1/4 thickness subjected to TMCP treatment |
![]() |