690 MPa级高强韧低碳微合金建筑结构钢设计及性能
|
|
Design and Performance of 690 MPa Grade Low-Carbon Microalloyed Construction Structural Steel with High Strength and Toughness
|
|
图 8. 实验用钢1/4厚度处的拉伸应力-应变曲线 |
Fig.8. Tensile stress-strain curve of the tested steel at 1/4 thickness |
![]() |