690 MPa级高强韧低碳微合金建筑结构钢设计及性能
|
|
Design and Performance of 690 MPa Grade Low-Carbon Microalloyed Construction Structural Steel with High Strength and Toughness
|
|
图 4. 实验用钢不同厚度处的SEM像 |
Fig.4. SEM images of the tested steel at different positions (LB—lath-like bainite, GB—granular bainite, BF—bainite ferrite, M/A—martensite/austenite) |
![]() |