大气条件下AlCrON基光谱选择性吸收涂层的热稳定性
|
|
Thermal Stability of AlCrON-Based Solar Selective Absorbing Coating in Air
|
|
图11. 大气条件下、500℃退火1000 h后AlCrON基光谱选择性吸收涂层截面的HAADF-STEM像和各元素的Mapping图 |
Fig.11. HAADF-STEM image and Mapping images of the distribution of elements in the AlCrON-based solar selective absorbing coating annealed at 500oC for 1000 h in air |
![]() |