大气条件下AlCrON基光谱选择性吸收涂层的热稳定性
|
|
Thermal Stability of AlCrON-Based Solar Selective Absorbing Coating in Air
|
|
图10. 大气条件下、500℃退火1000 h前后AlCrON基光谱选择性吸收涂层截面中各元素的EDS线扫描图 |
Fig.10. EDS line scan maps of the distribution of elements in the AlCrON-based solar selective absorbing coating before (a) and after (b) annealed at 500oC for 1000 h in air |
![]() |