大气条件下AlCrON基光谱选择性吸收涂层的热稳定性
|
|
Thermal Stability of AlCrON-Based Solar Selective Absorbing Coating in Air
|
|
图9. 大气条件下、500℃退火1000 h后AlCrON基光谱选择性吸收涂层中AlCrO减反射层的HRTEM像和FFT图与IFFT图 |
Fig.9. HRTEM image of the AlCrO anti-reflection layer after annealed at 500oC for 1000 h in air (a), and the corresponding FFT (b, d) and IFFT (c, e) images of areas I (b, c) and II (d, e) denoted in Fig.9a, respectively (Inset in Fig.9a shows the SAED pattern of the amorphous area, d(400) and d(202)—the spacings of (400) and (202) crystal planes, respectively) |
![]() |