大气条件下AlCrON基光谱选择性吸收涂层的热稳定性
|
|
Thermal Stability of AlCrON-Based Solar Selective Absorbing Coating in Air
|
|
图7. 大气条件下、500℃退火1000 h后AlCrON基光谱选择性吸收涂层中AlCrN吸收层的HRTEM像和FFT图与IFFT图 |
Fig.7. HRTEM image of the AlCrN absorbing layer after annealed at 500oC for 1000 h in air (a), and the corresponding fast Fourier transform (FFT) (b, d, f) and inverse fast Fourier transform (IFFT) (c, e, g) images of areas I (b, c), II (d, e), and III (f, g) denoted in Fig.7a, respectively (d(110)—spacing of (110) crystal plane) |
![]() |