大气条件下AlCrON基光谱选择性吸收涂层的热稳定性
|
|
Thermal Stability of AlCrON-Based Solar Selective Absorbing Coating in Air
|
|
图6. 大气条件下、500℃退火1000 h前后AlCrON基光谱选择性吸收涂层的TEM像和SAED花样 |
Fig.6. Bright field TEM images (a, c) and SAED patterns (b, d) of the AlCrON-based solar selective absorbing coating before (a, b) and after (c, d) annealed at 500oC for 1000 h in air |
![]() |