大气条件下AlCrON基光谱选择性吸收涂层的热稳定性
|
|
Thermal Stability of AlCrON-Based Solar Selective Absorbing Coating in Air
|
|
图1. 大气条件下、不同温度退火后AlCrON基光谱选择性吸收涂层的反射光谱 |
Fig.1. Reflectance spectra of the AlCrON-based solar selective absorbing coatings after annealed at 500oC (a) and 600oC (b) for different time in air |
![]() |