[an error occurred while processing this directive]
受BTA保护的白铜在模拟工业大气环境中的腐蚀行为
黄松鹏1,2, 彭灿1,2, 曹公望1,2, 王振尧1,2()
Corrosion Behavior of Copper-Nickel Alloys Protected by BTA in Simulated Urban Atmosphere
HUANG Songpeng1,2, PENG Can1,2, CAO Gongwang1,2, WANG Zhenyao1,2()

图9. BTA处理前后的白铜腐蚀336 h后的截面形貌高倍SEM像

Fig.9. High magnified cross section SEM images of copper-nickel alloys before (a) and after (b) BTA treatment after 336 h corrosion