受BTA保护的白铜在模拟工业大气环境中的腐蚀行为
黄松鹏1,2, 彭灿1,2, 曹公望1,2, 王振尧1,2()
Corrosion Behavior of Copper-Nickel Alloys Protected by BTA in Simulated Urban Atmosphere
HUANG Songpeng1,2, PENG Can1,2, CAO Gongwang1,2, WANG Zhenyao1,2()

. 图8不同腐蚀周期下BTA处理前后的白铜截面形貌的SEM像
(a1, b1) 48 h (a2, b2) 144 h (a3, b3) 240 h (a4, b4) 336 h

Fig.8. Cross section SEM images of copper-nickel alloys before (a1-a4) and after (b1-b4) BTA treatment in different corrosion time